Nhan đề: | Experimental Investigation on Dynamic Fracture Mechanism and Energy Evolution of Saturated Yellow Sandstone under Different Freeze-Thaw Temperatures |
Tác giả: | Chen, Liang Mao, Xianbiao Yang, Shengli Chao, An Wu, Peng |
Từ khoá: | Mechanical properties Cold Impact tests Compression tests Stress-strain curves Sandstone Disasters Nonferrous metals Mechanics Fracture mechanics Storage modulus Dynamic loads High speed cameras Design engineering Temperature Failure Energy dissipation Civil engineering Stone Design optimization |
Năm xuất bản: | 2019 |
Nhà xuất bản: | Hindawi Limited |
Tóm tắt: | The coupling effect of freeze-thaw (F-T) temperature and dynamic load on the dynamic mechanical properties and fracture mechanism of saturated yellow sandstone was experimentally investigated in this research. The dynamic compression tests on the specimen after different F-T temperatures (i.e., −5°С, −10°С, −15°С, −20°С, −30°С, and 20°С) have been carried out with split-Hopkinson pressure bar (SHPB) setup under eight F-T cycle numbers. The density and P-wave velocity of the specimens were obtained before and after the F-T tests. After the F-T tests, the specimen microstructures were examined via the scanning electron microscope (SEM). The dynamic fracture process was visualized by the high-speed camera. The particle size distribution and fragment shapes of the specimens were analyzed using a classifying screen. In addition, the energy dissipation law of specimens during the impact test was also discussed. Experimental results show that the dynamic elastic modulus, strength of the specimen, and the average particle size decrease with decreasing F-T temperature. SEM results reveal that low F-T temperature leads to severer internal damage of the specimen by inducing freeze-swell holes, interconnected cracks, and pore clusters. In addition, the fragmentation shapes of the failed specimens exhibit double-cone failure, single-side slope failure, double-side slope failure, and split failure. The energy dissipation increases gradually with increasing F-T temperature. This study helps to prevent geological disasters and optimize engineering design in cold regions. |
Mô tả: | Advances in Civil Engineering; New York Vol. 2019, (2019). DOI:10.1155/2019/2375276 |
Định danh: | http://thuvienso.vanlanguni.edu.vn/handle/Vanlang_TV/18470 |
ISSN: | 1687-8086 1687-8094 (eISSN) |
Bộ sưu tập: | Bài báo_lưu trữ |
Các tập tin trong tài liệu này:
Tập tin | Mô tả | Kích thước | Định dạng | |
---|---|---|---|---|
BBKH1192_TCCN_Experimental Investigation on ....pdf Giới hạn truy cập | Experimental Investigation on Dynamic Fracture Mechanism and Energy Evolution of Saturated Yellow Sandstone under Different Freeze-Thaw Temperatures | 7.24 MB | Adobe PDF | Xem/Tải về Yêu cầu tài liệu |
Khi sử dụng các tài liệu trong Thư viện số phải tuân thủ Luật bản quyền.